Nickel alloys are used where stainless steels run out of corrosion or temperature resistance. With 30–99 % nickel and additions of chromium, molybdenum, copper or tungsten, they resist strong acids, chlorides, caustics and oxidation from cryogenic temperatures to above 1000 °C.
What nickel alloys is
They are often known by trade names: Inconel 600 and 625 (nickel–chromium), Incoloy 800H and 825 (nickel–iron–chromium), Hastelloy C-276 and C-22 (nickel–molybdenum–chromium) and Monel 400 (nickel–copper). In ASTM, forged flanges and fittings are covered by B564, butt-weld fittings by B366, and pipe and plate by alloy-specific specifications.
- Nickel 30–99 %
- Chromium for oxidising media (600, 625, 825, C-22)
- Molybdenum for reducing acids and pitting (625, C-276, C-22)
- Copper for sulphuric acid and seawater (825, 400)
- Supplied annealed or solution annealed
Key properties
| PREN of Alloy 625 / C-276 | ≈ 50 / ≈ 68 |
|---|---|
| Minimum yield (B564 annealed) | 172 MPa (Alloy 400) – 414 MPa (Alloy 625) |
| Temperature range | Cryogenic to above 1000 °C (600, 800H) |
| Chloride stress-corrosion cracking | Essentially immune above about 40 % Ni |
Nickel alloys grades compared
Chemistry and minimum room-temperature properties from the governing ASTM / ASME / API specifications. Open any grade for its full data sheet and PDF.
| Grade | Form | UNS | Cr% | Ni% | Mo% | C% | YieldMPa min | TensileMPa min |
|---|---|---|---|---|---|---|---|---|
| Alloy 625 (UNS N06625) | Nickel alloy forgings, fittings & pipe | N06625 | 20.0–23.0 | 58.0 min | 8.0–10.0 | 0.10 max | 414 | 827 |
| Alloy 600 (UNS N06600) | Nickel alloy forgings, fittings & pipe | N06600 | 14.0–17.0 | 72.0 min | — | 0.15 max | 240 | 550 |
| Alloy 825 (UNS N08825) | Nickel alloy forgings, fittings & pipe | N08825 | 19.5–23.5 | 38.0–46.0 | 2.5–3.5 | 0.05 max | 241 | 586 |
| Alloy 800 / 800H / 800HT | Nickel alloy forgings, fittings & pipe | N08800 / N08810 / N08811 | 19.0–23.0 | 30.0–35.0 | — | 0.10 max (800), 0.05–0.10 (800H), 0.06–0.10 (800HT) | 207 | 517 |
| Alloy C-276 (UNS N10276) | Nickel alloy forgings, fittings & pipe | N10276 | 14.5–16.5 | balance | 15.0–17.0 | 0.010 max | 283 | 690 |
| Alloy C-22 (UNS N06022) | Nickel alloy forgings, fittings & pipe | N06022 | 20.0–22.5 | balance | 12.5–14.5 | 0.015 max | 310 | 690 |
| Alloy 400 (UNS N04400) | Nickel-copper forgings, fittings & pipe | N04400 | — | 63.0 min (incl. Co) | — | 0.3 max | 172 | 483 |
| Nickel 200 / 201 (UNS N02200 / N02201) | Pure nickel forgings, fittings & pipe | N02200 / N02201 | — | 99.0 min | — | 0.15 max (200), 0.02 max (201) | 105 | 380 |
Reference information compiled from the published standard for convenience. It does not replace the current edition of the governing standard, which takes precedence. Verify critical dimensions and properties before design, purchase or fabrication. Teshi Engineers & Sales Promoters (P) Ltd accepts no liability for errors or omissions.
Specifications by product form
| Product form | Grades |
|---|---|
| Nickel alloy forgings, fittings & pipe | Alloy 625 (UNS N06625), Alloy 600 (UNS N06600), Alloy 825 (UNS N08825), Alloy 800 / 800H / 800HT, Alloy C-276 (UNS N10276), Alloy C-22 (UNS N06022) |
| Nickel-copper forgings, fittings & pipe | Alloy 400 (UNS N04400) |
| Pure nickel forgings, fittings & pipe | Nickel 200 / 201 (UNS N02200 / N02201) |
Where nickel alloys is used
- Sour gas, flare and offshore process lines
- Flue-gas desulphurisation and chemical scrubbers
- Sulphuric, hydrochloric and hydrofluoric acid service
- Reformer, cracker and furnace piping (800H/800HT)
- Seawater and marine hardware (625, 400)
Welding and fabrication
Nickel alloys are welded with matching or over-alloyed ERNi consumables, low heat input and strict cleanliness — sulphur and lead contamination cause cracking. Preheat is not normally required. PMI on every piece and certification to EN 10204 3.1 or 3.2 are standard.
FAQ
Nickel alloys: common questions
What is the difference between Inconel 625 and Incoloy 825?
Alloy 625 (N06625) is about 60 % nickel with 9 % molybdenum and niobium — stronger and far more resistant to pitting. Alloy 825 (N08825) is a nickel–iron–chromium alloy with copper and titanium, designed for sulphuric and phosphoric acid at lower cost.
Which ASTM specification covers nickel alloy flanges?
ASTM B564 covers nickel alloy forgings, including flanges and forged fittings. Butt-weld fittings are covered by ASTM B366.
What is Hastelloy C-276 used for?
Severe reducing and mixed-acid service — wet chlorine, hypochlorite, hydrochloric acid and FGD scrubbers — where even 6Mo stainless steels fail.
Nickel alloys products from Teshi Group
Inconel 600, 625 & 825 Flanges & Fittings
Grades, sizes and standards we supply
ViewMaterial productsInconel 625 Flanges
Grades, sizes and standards we supply
ViewMaterial productsInconel 600 / Incoloy 825 Flanges
Grades, sizes and standards we supply
ViewMaterial productsInconel 625 Pipe Fittings
Grades, sizes and standards we supply
ViewMaterial productsHastelloy C-276 / C-22 Flanges
Grades, sizes and standards we supply
ViewMaterial productsHastelloy C-276 Pipe Fittings
Grades, sizes and standards we supply
ViewMaterial productsMonel 400 Flanges
Grades, sizes and standards we supply
ViewMaterial productsMonel 400 Pipe Fittings
Grades, sizes and standards we supply
ViewMaterial productsHastelloy C-276, C-22, Monel 400 & Alloy 20 Flanges & Fittings
Grades, sizes and standards we supply
ViewOEM manufacturerIndustrial Flanges
ViewOEM manufacturerButt Weld Fittings
ViewStockist & supplierIndustrial Pipes
View
Ready to build to spec?
Share your drawing, bill of materials or technical requirements with the Teshi team.