ISO 9001:2015IBR ApprovedEstablished 1971Full Material Traceability
GroupRequest a quote
Material family8 grade data sheets

Low-temperature carbon steel (LTCS) & 3.5 % nickel grades

Low-temperature carbon steel (LTCS) is carbon–manganese steel with fine-grain practice and heat treatment chosen to keep its toughness in cold service. Every heat is Charpy impact-tested at the minimum design temperature, which is what separates LTCS from ordinary carbon steel.

What low-temperature carbon steel (ltcs) is

Standard LTCS grades (A350 LF2, A420 WPL6, A333 Gr 6, A352 LCB/LCC) are impact-tested at −46 °C. For colder service down to −101 °C, 3.5 % nickel steels are used: A350 LF3, A420 WPL3 and A333 Gr 3.

  • Carbon 0.30 % max, manganese up to 1.35 %
  • Fine-grain, killed steel; normalised or quenched and tempered
  • Mandatory Charpy V-notch testing at −46 °C (LF2/WPL6) or −101 °C (LF3/WPL3)
  • 3.5 % nickel added in LF3 and WPL3 for lower temperatures

Key properties

LF2 / WPL6 / A333-6 impact test−46 °C
LF3 / WPL3 impact test−101 °C
Typical minimum yield240–275 MPa
Typical minimum tensile415–485 MPa
ASME B16.5 material group1.1 (LF2), 1.2 (LF3)

Low-temperature carbon steel (LTCS) grades compared

Chemistry and minimum room-temperature properties from the governing ASTM / ASME / API specifications. Open any grade for its full data sheet and PDF.

GradeFormUNSCr%Ni%Mo%C%YieldMPa minTensileMPa min
ASTM A350 LF2 Cl.1Forged flanges & fittingsK030110.30 max0.40 max0.12 max0.30 max250485
ASTM A420 WPL6Wrought butt-weld fittingsK030060.30 max0.40 max0.12 max0.30 max240415
ASTM A350 LF3 Cl.1Forged flanges & fittingsK320250.30 max3.3–3.70.12 max0.20 max260485
ASTM A333 Grade 6Seamless & welded pipeK03006———0.30 max240415
ASTM A420 WPL3Wrought butt-weld fittings——3.2–3.8—0.20 max240450
ASTM A352 LCBLow-temperature steel castingsJ03003———0.30 max240450
ASTM A352 LCCLow-temperature steel castingsJ02505———0.25 max275485
ASTM A333 Grade 3Seamless & welded pipeK31918—3.18–3.82—0.19 max240450

Reference information compiled from the published standard for convenience. It does not replace the current edition of the governing standard, which takes precedence. Verify critical dimensions and properties before design, purchase or fabrication. Teshi Engineers & Sales Promoters (P) Ltd accepts no liability for errors or omissions.

Specifications by product form

Product formGrades
Forged flanges & fittingsASTM A350 LF2 Cl.1, ASTM A350 LF3 Cl.1
Wrought butt-weld fittingsASTM A420 WPL6, ASTM A420 WPL3
Seamless & welded pipeASTM A333 Grade 6, ASTM A333 Grade 3
Low-temperature steel castingsASTM A352 LCB, ASTM A352 LCC

Where low-temperature carbon steel (ltcs) is used

  • LNG and LPG terminals and storage
  • Ethylene and refrigeration plants
  • Gas processing and dehydration units
  • Cold-climate and arctic pipelines
  • Blowdown and depressurisation lines that chill on venting

Welding and fabrication

Weld procedures for LTCS must be impact-qualified at the design temperature, with controlled heat input. Post-weld heat treatment is common for thicker sections. Keep consumables and procedures matched to the grade (e.g. E7018-1 for LF2, nickel-bearing consumables for LF3).

FAQ

Low-temperature carbon steel (LTCS): common questions

What temperature is LTCS good for?

Standard LTCS grades such as A350 LF2 Cl.1 and A333 Gr 6 are impact-tested at −46 °C. For service down to −101 °C, 3.5 % nickel grades such as A350 LF3 are used.

What is the difference between A350 LF2 Class 1 and Class 2?

Both have the same chemistry and strength; Class 1 is impact-tested at −46 °C and Class 2 at −18 °C.

Which LTCS grades go together?

A333 Gr 6 pipe, A420 WPL6 butt-weld fittings, A350 LF2 flanges, A352 LCB/LCC valves and A320 L7 bolting with A194 Gr 7 nuts.

Ready to build to spec?

Share your drawing, bill of materials or technical requirements with the Teshi team.