ISO 9001:2015IBR ApprovedEstablished 1971Full Material Traceability
GroupRequest a quote
Material family34 grade data sheets

Austenitic stainless steel grades — 304, 316, 321, 347, 310

Austenitic stainless steels are iron–chromium–nickel alloys with 16–26 % chromium and 8–22 % nickel. Nickel keeps the structure austenitic (face-centred cubic), which makes these steels non-magnetic when annealed, very tough down to cryogenic temperatures, and easy to form and weld.

What austenitic stainless steel is

The 300-series family covers most stainless piping: 304/304L for general corrosion, 316/316L with molybdenum for chlorides, 321 and 347 stabilised against sensitisation, H grades for high-temperature strength, 317L for more aggressive chemicals, and 310/310S for oxidation resistance up to about 1100 °C.

  • Chromium 16–26 % and nickel 8–22 %
  • L grades: carbon 0.030–0.035 % max to avoid sensitisation when welded
  • H grades: carbon 0.04–0.10 % for creep strength above about 525 °C
  • Ti- or Nb-stabilised grades (321, 347, 316Ti) tie up carbon as carbides
  • Molybdenum 2–4 % in 316/317 for pitting resistance

Key properties

Minimum yield (annealed)170 MPa (L grades) – 205 MPa
Minimum tensile485–515 MPa
ToughnessExcellent down to −196 °C (cryogenic)
MagneticNon-magnetic when annealed
ASME B16.5 material groups2.1 (304), 2.2 (316), 2.3 (304L/316L), 2.4 (321), 2.5 (347), 2.11 (310)

Austenitic stainless steel grades compared

Chemistry and minimum room-temperature properties from the governing ASTM / ASME / API specifications. PREN = Cr + 3.3Mo + 16N using specification minimums. Open any grade for its full data sheet and PDF.

GradeFormUNSCr%Ni%Mo%N%PRENminYieldMPa minTensileMPa min
ASTM A182 F304Forged flanges & fittingsS3040018.0–20.08.0–11.0—0.10 max18205515
ASTM A182 F304LForged flanges & fittingsS3040318.0–20.08.0–13.0—0.10 max18170485
ASTM A182 F316Forged flanges & fittingsS3160016.0–18.010.0–14.02.00–3.000.10 max23205515
ASTM A182 F316LForged flanges & fittingsS3160316.0–18.010.0–15.02.00–3.000.10 max23170485
ASTM A182 F321Forged flanges & fittingsS3210017.0–19.09.0–12.0——17205515
ASTM A312 TP304Seamless pipe (seamless & welded)S3040018.0–20.08.0–11.0——18205515
ASTM A312 TP304LSeamless pipe (seamless & welded)S3040318.0–20.08.0–13.0——18170485
ASTM A312 TP316Seamless pipe (seamless & welded)S3160016.0–18.010.0–14.02.00–3.00—23205515
ASTM A312 TP316LSeamless pipe (seamless & welded)S3160316.0–18.010.0–14.02.00–3.00—23170485
ASTM A403 WP304Wrought butt-weld fittingsS3040018.0–20.08.0–11.0——18205515
ASTM A403 WP304LWrought butt-weld fittingsS3040318.0–20.08.0–12.0——18170485
ASTM A403 WP316Wrought butt-weld fittingsS3160016.0–18.010.0–14.02.00–3.00—23205515
ASTM A403 WP316LWrought butt-weld fittingsS3160316.0–18.010.0–14.02.00–3.00—23170485
ASTM A351 CF8MAustenitic steel castingsJ9290018.0–21.09.0–12.02.0–3.0—25205485
ASTM A182 F304HForged flanges & fittingsS3040918.0–20.08.0–11.0——18205515
ASTM A182 F316HForged flanges & fittingsS3160916.0–18.010.0–14.02.00–3.00—23205515
ASTM A182 F316TiForged flanges & fittingsS3163516.0–18.010.0–14.02.00–3.000.10 max23205515
ASTM A182 F317LForged flanges & fittingsS3170318.0–20.011.0–15.03.0–4.0—28170485
ASTM A182 F310Forged flanges & fittingsS3100024.0–26.019.0–22.0——24205515
ASTM A182 F321HForged flanges & fittingsS3210917.0–19.09.0–12.0——17205515
ASTM A182 F347Forged flanges & fittingsS3470017.0–20.09.0–13.0——17205515
ASTM A182 F347HForged flanges & fittingsS3470917.0–20.09.0–13.0——17205515
ASTM A312 TP304HSeamless & welded pipeS3040918.0–20.08.0–11.0——18205515
ASTM A312 TP316HSeamless & welded pipeS3160916.0–18.011.0–14.02.00–3.00—23205515
ASTM A312 TP321Seamless & welded pipeS3210017.0–19.09.0–12.0—0.10 max17205515
ASTM A312 TP347Seamless & welded pipeS3470017.0–19.09.0–13.0——17205515
ASTM A312 TP310SSeamless & welded pipeS3100824.0–26.019.0–22.00.75 max—24205515
ASTM A312 TP317LSeamless & welded pipeS3170318.0–20.011.0–15.03.0–4.0—28205515
ASTM A403 WP321Wrought butt-weld fittingsS3210017.0–19.09.0–12.0—0.10 max17205515
ASTM A403 WP347Wrought butt-weld fittingsS3470017.0–19.09.0–13.0——17205515
ASTM A403 WP310SWrought butt-weld fittingsS3100824.0–26.019.0–22.00.75 max—24205515
ASTM A403 WP317LWrought butt-weld fittingsS3170318.0–20.011.0–15.03.0–4.0—28205515
ASTM A351 CF8Austenitic steel castingsJ9260018.0–21.08.0–11.00.50 max—18205485
ASTM A351 CF3MAustenitic steel castingsJ9280017.0–21.09.0–13.02.0–3.0—24205485

Reference information compiled from the published standard for convenience. It does not replace the current edition of the governing standard, which takes precedence. Verify critical dimensions and properties before design, purchase or fabrication. Teshi Engineers & Sales Promoters (P) Ltd accepts no liability for errors or omissions.

Where austenitic stainless steel is used

  • Chemical, pharmaceutical and food processing
  • Cryogenic LNG and air-separation plants
  • Refinery and petrochemical process lines
  • Water treatment and desalination pre-treatment
  • High-temperature furnace and heater piping (H, 321, 347, 310 grades)

Welding and fabrication

Austenitic grades weld readily with matching consumables (308L, 316L, 347, 309/310). Use L or stabilised grades for welded equipment that must resist intergranular corrosion. They are prone to chloride stress-corrosion cracking above about 60 °C — duplex or super austenitic grades are preferred there. Dual-certified material (e.g. 316/316L) is common.

FAQ

Austenitic stainless steel: common questions

What is the difference between 316 and 316L?

316L has carbon 0.030 % max against 0.08 % for 316. The lower carbon prevents chromium-carbide precipitation in weld heat-affected zones, so 316L keeps its corrosion resistance after welding. 316L has slightly lower minimum strength (170 vs 205 MPa yield); dual-certified 316/316L meets both.

When should I use 321 or 347 instead of 304L?

For service between about 425 °C and 815 °C, where low-carbon grades lose strength and plain grades sensitise. Titanium (321) or niobium (347) stabilises the carbon.

What are H grades used for?

304H, 316H, 321H and 347H have controlled 0.04–0.10 % carbon and a coarse grain size for higher creep strength above about 525 °C.

Is austenitic stainless steel magnetic?

Not in the annealed condition. Cold work can make 304 and 316 slightly magnetic.

Ready to build to spec?

Share your drawing, bill of materials or technical requirements with the Teshi team.