Titanium Grade 7 (UNS R52400) — Chemical Composition & Mechanical Properties

Titanium Grade 7 (UNS R52400) is a titanium grade for titanium forgings, fittings & pipe (UNS R52400, EN / W.Nr 3.7235). It is also known as Ti-0.15Pd. This sheet summarises its chemical composition limits, minimum mechanical properties, heat treatment and typical service. Teshi Group manufactures flanges and fittings in this grade.

Download PDF Request a quoteA4 · Teshi Group document TG-MG-095 · © Teshi Group · controlled document

Titanium Grade 7 (UNS R52400) at a glance

SpecificationTitanium Grade 7 (UNS R52400)
Material familyTitanium
Product formTitanium forgings, fittings & pipe
UNS numberR52400
EN / W.Nr equivalent3.7235
Also known asTi-0.15Pd
DocumentTG-MG-095 · Rev. 1 · October 2026

Typical service

Reducing acids and hot brine where Grade 2 would suffer crevice corrosion

Heat treatment

Annealed

Chemical composition of Titanium Grade 7 (UNS R52400) (weight %)

Tibalance
Pd0.12–0.25
O0.25 max
Fe0.30 max
C0.08 max
N0.03 max
H0.015 max

Single values are maximums unless shown as a range or “min”.

Mechanical properties

Tensile strength, min345 MPa
Yield strength (0.2 % offset), min275 MPa
Elongation, min20 %
Yield strength, max450 MPa
HardnessNot specified

About titanium

Titanium forms a stable oxide film that makes it practically immune to seawater, chlorides, wet chlorine and many oxidising acids. It is about 45 % lighter than steel for similar strength, which matters offshore and in heat-exchanger service.

Reference information compiled from the published standard for convenience. It does not replace the current edition of the governing standard, which takes precedence. Verify critical dimensions and properties before design, purchase or fabrication. Teshi Engineers & Sales Promoters (P) Ltd accepts no liability for errors or omissions.

International equivalents of Titanium Grade 7 (UNS R52400)

All equivalents
Standard systemNearest equivalent grade
USA — specificationTitanium Grade 7 (UNS R52400)
USA — UNSR52400
Europe — EN designationTi Grade 7 (Ti-0.15Pd)
Europe — W.Nr3.7235
Japan — JISTTP340Pd / Class 12 (JIS H4630)
China — GB / NBTA9 (GB/T 3624)
China — old GB designationTA9

Equivalents are the nearest commonly cited grades. Chemistry, mechanical properties and testing differ between standards — compare them before substituting one for another.

Same alloy in other product forms

Product formSpecification / grade
Flanges & forgingsASTM B381 F-7
Butt-weld fittingsASTM B363 WPT7
Seamless pipeASTM B861 Grade 7
Welded pipeASTM B862 Grade 7
PlateASTM B265 Grade 7
BarASTM B348 Grade 7

FAQ

Titanium Grade 7 (UNS R52400): common questions

What is the minimum yield strength of Titanium Grade 7 (UNS R52400)?

275 MPa, with a minimum tensile strength of 345 MPa.

What is the carbon content of Titanium Grade 7 (UNS R52400)?

0.08 max %.

What is the UNS number and EN equivalent of Titanium Grade 7 (UNS R52400)?

UNS R52400; the nearest European designation is W.Nr 3.7235. Equivalents are close but not identical — check the specification if substituting.

How is Titanium Grade 7 (UNS R52400) heat treated?

Annealed.

What is the Chinese (GB) equivalent of Titanium Grade 7 (UNS R52400)?

The nearest Chinese equivalent is TA9 (GB/T 3624), formerly TA9. Equivalents are close but not identical — compare chemistry and properties before substituting.

What is the JIS equivalent of Titanium Grade 7 (UNS R52400)?

The nearest Japanese (JIS) equivalent is TTP340Pd / Class 12 (JIS H4630).

Does Teshi Group supply Titanium Grade 7 (UNS R52400)?

Teshi Group manufactures flanges and fittings in this grade. Send your size, rating and quantity to info@teshigroup.com for a quotation with EN 10204 3.1 certificates.

Ready to build to spec?

Share your drawing, bill of materials or technical requirements with the Teshi team.