ISO 9001:2015IBR ApprovedEstablished 1971Full Material Traceability
GroupRequest a quote
Chrome-molyAlloy steel castingsTG-MG-123 · Rev. 1 · October 2026

ASTM A217 WC9 — Chemical Composition & Mechanical Properties

ASTM A217 WC9 is a chrome-moly alloy steel grade for alloy steel castings (UNS J21890, EN / W.Nr ≈ 1.7379). It is also known as 2¼Cr-1Mo cast. This sheet summarises its chemical composition limits, minimum mechanical properties, heat treatment and typical service. Teshi Group manufactures valves with bodies in this grade.

Download PDF Request a quoteA4 · Teshi Group document TG-MG-123 · © Teshi Group · controlled document

ASTM A217 WC9 at a glance

SpecificationASTM A217 WC9
Material familyChrome-moly alloy steel
Product formAlloy steel castings
UNS numberJ21890
EN / W.Nr equivalent≈ 1.7379
Also known as2¼Cr-1Mo cast
DocumentTG-MG-123 · Rev. 1 · October 2026

Typical service

High-temperature steam valve bodies (2¼Cr-1Mo)

Heat treatment

Normalised and tempered 675 °C min

Chemical composition of ASTM A217 WC9 (weight %)

C0.05–0.18
Mn0.40–0.70
P0.04 max
S0.045 max
Si0.60 max
Cr2.00–2.75
Mo0.90–1.20

Single values are maximums unless shown as a range or “min”.

Mechanical properties

Tensile strength, min485 MPa
Yield strength (0.2 % offset), min275 MPa
Elongation, min20 %
HardnessNot specified

About chrome-moly alloy steel

Chrome-moly steels are low-alloy steels with 1–9 % chromium and 0.5–1 % molybdenum. Chromium gives oxidation and sulphidation resistance; molybdenum gives creep strength at high temperature. They are the standard choice for steam and hot hydrocarbon service above the carbon-steel range.

Reference information compiled from the published standard for convenience. It does not replace the current edition of the governing standard, which takes precedence. Verify critical dimensions and properties before design, purchase or fabrication. Teshi Engineers & Sales Promoters (P) Ltd accepts no liability for errors or omissions.

International equivalents of ASTM A217 WC9

All equivalents
Standard systemNearest equivalent grade
USA — ASTM / ASMEASTM A217 WC9 · ASME SA-217 WC9
USA — UNSJ21890
Europe — EN designationG17CrMo9-10 (EN 10213)
Europe — W.Nr1.7379
Japan — JISSCPH32 (JIS G5151)
China — GB / NBWC9 (GB/T 12229) / ZG12Cr2Mo1
UK — BS (withdrawn)BS 1504-622

Equivalents are the nearest commonly cited grades. Chemistry, mechanical properties and testing differ between standards — compare them before substituting one for another.

FAQ

ASTM A217 WC9: common questions

What is the minimum yield strength of ASTM A217 WC9?

275 MPa, with a minimum tensile strength of 485 MPa.

What is the carbon content of ASTM A217 WC9?

0.05–0.18 %.

What is the UNS number and EN equivalent of ASTM A217 WC9?

UNS J21890; the nearest European designation is W.Nr ≈ 1.7379. Equivalents are close but not identical — check the specification if substituting.

How is ASTM A217 WC9 heat treated?

Normalised and tempered 675 °C min.

What is the Chinese (GB) equivalent of ASTM A217 WC9?

The nearest Chinese equivalent is WC9 (GB/T 12229) / ZG12Cr2Mo1. Equivalents are close but not identical — compare chemistry and properties before substituting.

What is the JIS equivalent of ASTM A217 WC9?

The nearest Japanese (JIS) equivalent is SCPH32 (JIS G5151).

Does Teshi Group supply ASTM A217 WC9?

Teshi Group manufactures valves with bodies in this grade. Send your size, rating and quantity to info@teshigroup.com for a quotation with EN 10204 3.1 certificates.

Ready to build to spec?

Share your drawing, bill of materials or technical requirements with the Teshi team.